Pop-Outs in Concrete
Pop-outs Diagnosis: Also known as rock-pops, they are small cone-shaped pieces of a concrete surface that separate due to focused internal pressure. Small pop-outs leave holes up to 0.4 in. …
Pop-outs Diagnosis: Also known as rock-pops, they are small cone-shaped pieces of a concrete surface that separate due to focused internal pressure. Small pop-outs leave holes up to 0.4 in. …
Alkali-Silica Reaction (ASR), the reaction between alkalies in portland cement and certain siliceous rocks or minerals Diagnosis: An expansive cracking condition with discoloration. Cause: A chemical reaction between the naturally …
Delamination of Concrete Diagnosis: Delamination is a separation, splitting or de-bonding of the concrete’s thickness along a plane parallel to the surface. Spotted visually if the deterioration is advanced or …
Concrete Honeycombing Cause: Failure of the cement paste to consolidate and fill the voids between the more coarse aggregates. Possible concrete repair solutions: Functional/aesthetic concrete only: Chip by hand to …
Plastic Shrinkage Cracking in Concrete Materials Cause: Plastic Shrinkage Cracking occurs as a result of very rapid evaporation of the concrete while it is still in a plastic state. Hot, …
Crazing Diagnosis: Random fine cracking on the surface resembling cracked mud on a dried up pond, but in a smaller pattern. Prevention: Any concrete or masonry surface can be subject …
Bug Holes Diagnosis: Also known as blow-holes, bug-holes are small air-bubble voids on the surface of formed concrete. Cause: Air entrapped during concrete placement and consolidation. Three main factors contribute …